Fusion between the steel sheet and glass coating is very important Glass-Fused-to-Steel tanks production steps because it directly affects the Glass-Fused-to-Steel tank service life. In order to provide a high-quality product to our clients, Shijiazhuang Zhengzhong Technology Co.,Ltd conduct very strict quality control from raw material to final product. Before mass production, raw material and small sample test need to be done to check the quality of raw material and fusion between coating and steel panel, if qualified then mass production will be carried out. Tanks are produced on the automatic production line, to make sure good and stable quality control. After the production all steel panels need to be tested by 1500V spark holiday test, all steel panels are 0 discontinuity.

CNC Laser Cutting

Inputting the Confirmed drawing into the computer, bolt holes and openings will be cut by CNC laser cutting machine automatically.

التحضير المسبق للصلب - المعالجة بالرش

الانحناء بشكل قوس

المعالجة بالرش وفقًا للمواصفة SSPC SP10 ، سطح الصلب ذو لون فضي

بعد المعالجة بالرش ، يجب أن يتم انحناء لوح الصلب بشكل قوسي وفقًا لقطر الخزان.

رش الطلاء التلقائي للمينا

رش الإيناميل التلقائي على كلا الجانبين من المعدن. يتم التحكم في سمك الطبقة بين 230 و 450 ميكرومتر.

فرن الانفجار عالي الحرارة

بعد التطبيق والتجفيف ، تنصهر سطح ورقة الصلب بين المكونين عند حرارة تتراوح بين 820 درجة مئوية و 930 درجة مئوية في الفرن.

مراجعة المنتج

يجب أن يتم التحكم في جودة الإنتاج بعد الإنتاج. يتضمن ذلك فحص سمك الطلاء ، واختبار الختم ، وتوافق الألوان وما إلى ذلك.